Biomechanical and histomorphometric study on the bone-screw interface of bioactive ceramic-coated titanium screws

DC Field Value Language
dc.contributor.authorLee, Jae Hyup-
dc.contributor.authorRyu, Hyun-Seung-
dc.contributor.authorLee, Dong-Soo-
dc.contributor.authorHong, Kug Sun-
dc.contributor.authorChang, Bong-Soon-
dc.contributor.authorLee, Choon-Ki-
dc.date.accessioned2009-11-13T07:02:07Z-
dc.date.available2009-11-13T07:02:07Z-
dc.date.issued2005-
dc.identifier.citationBiomaterials 2005;26:3249-57en
dc.identifier.issn0142-9612 (Print)-
dc.identifier.urihttp://www.ncbi.nlm.nih.gov/entrez/query.fcgi?cmd=Retrieve&db=PubMed&dopt=Citation&list_uids=15603820-
dc.identifier.urihttps://hdl.handle.net/10371/12145-
dc.description.abstractThe purpose of this study was to compare the osseointegration of 4 different kinds of bioactive ceramic-coated screws with uncoated screws by biomechanical and histomorphometric analysis. Calcium pyrophosphate (CPP), apatite-wollastonite 1:3 glass ceramic (W3G), apatite-wollastonite 1:1 glass ceramic (WAG) and bioactive CaO-SiO2-B2O3 glass ceramic (CSG) coatings were prepared and coated by the dipping method. Coated and uncoated titanium screws were inserted into the tibia of 18 adult mongrel male dogs for 2, 4, and 8 weeks. The insertion torques, radiographs, undecalcified histology, histomorphometric analysis, and extraction torques were evaluated. No difference of insertion torque was found among the five screw types. At 2 and 4 weeks after implantation, the extraction torque of ceramic-coated screws was significantly higher than that of uncoated screws (p < or = 0.0001). At 8 weeks, the extraction torques of CPP-, W3G-, and WAG-coated screws were significantly higher than those of CSG-coated and uncoated screws (p<0.0001). At 2, 4, and 8 weeks, the extraction torques of 4 different ceramic-coated screws were significantly higher than the corresponding insertion torque. Strong fixation was observed even at 2 weeks in the CPP-, W3G- and WAG-coated screws. The bone-screw contacts of the 4 different coated screws at 2 and 4 weeks were statistically higher than that of the uncoated screws, and the bone-screw contacts of the CPP-, W3G- and WAG-coated screws at 8 weeks were also statistically higher than that of the uncoated screws. The fixation strength was increased by the presence of osteoconductive coating materials, such as CPP, W3G, and WAG, which enabled to achieve higher fixation strength even as early as 2-8 weeks after the insertion.en
dc.description.sponsorshipsupported by a Grant-in-Aid for
Common core technology development programs from the KoreanMinistry of Commerce, Industry and Energy
(No. A00-A01-3302-02-1-3).
en
dc.language.isoen-
dc.publisherElsevieren
dc.subjectBioactive ceramicen
dc.subjectCoatingen
dc.subjectTitanium screwen
dc.subjectOsseointegrationen
dc.subjectBiomechanicalen
dc.subjectHistomorphometric analysisen
dc.titleBiomechanical and histomorphometric study on the bone-screw interface of bioactive ceramic-coated titanium screwsen
dc.typeArticleen
dc.contributor.AlternativeAuthor이재협-
dc.contributor.AlternativeAuthor류현승-
dc.contributor.AlternativeAuthor이동수-
dc.contributor.AlternativeAuthor홍국선-
dc.contributor.AlternativeAuthor장봉순-
dc.contributor.AlternativeAuthor이춘기-
dc.identifier.doi10.1016/j.biomaterials.2004.08.033-
Appears in Collections:
Files in This Item:
There are no files associated with this item.

Altmetrics

Item View & Download Count

  • mendeley

Items in S-Space are protected by copyright, with all rights reserved, unless otherwise indicated.

Share