Publications

Detailed Information

A new manufacturing method of all ceramic restoration using alumina tape and presentation of clinical cases

Cited 0 time in Web of Science Cited 0 time in Scopus
Authors

Oh, Nam-Sik; Kim, Eui-Seong; Lee, Keun-Woo; Han, Jung-Suk; Kim, Dae-Joon; Lee, Myung-Hyun

Issue Date
2000
Publisher
대한치과보철학회
Citation
2000;38(6)
Keywords
All ceramic crownalumina tapeflexure strengthfithess
Abstract
in an effort to facilitate fabrication procedure of all ceramic crowns, a novel preparation method for all ceramic crown using alumina tape was developed. The alumina tape having a uniform thickness was cast by using Doctor blade method. The physical properties of newly introduced alumina tape has biaxial flexure strength of . The value of toughness is which corelates with fracture and the linear shrinkage rate of the alumina tape is 0.44% during core production. The marginal fitness of the alumina tape all-ceramic restoration with shoulder margin had average marginal discrepancy at > and average marginal gap at >. At the marginal preparation of deep chamfer, the average marginal discrepancy at > and the average marginal gap at > had been reported. This fabrication procedure of all ceramic crowns with alumina tapes is easier and less technical sensitive for dental technicians. After restoration with new all ceramic crowns we followed the patients 2 years later, there were no complications as porcelain fractures or periodontal disease. We had good esthetic clinical results with new all ceramic crowns.
ISSN
0301-2875
Language
English
URI
https://hdl.handle.net/10371/47697
Files in This Item:
Appears in Collections:

Altmetrics

Item View & Download Count

  • mendeley

Items in S-Space are protected by copyright, with all rights reserved, unless otherwise indicated.

Share