dc.description.abstractEnamel microabrasion is a means by which superficial enamel discoloration is removed using hydrochloric acid and fine pumice. As enamel microabrasion alone may not be sufficient in cases of deeper discoloration, composite resin restoration is recommended in areas where there is remaining discoloration. The purpose of this study was to investigate the effects of different methods and number of applications of enamel microabrasion on the shear bond strength of composite resin to enamel. Untreated control was designated as group 1. 5-second applications of a mixture of 18% HCl and fine pumice were performed 5 and 10 times on groups 2 and 3, respectively. A commercially available mixture of 10% HCl and abrasives(PREMA) was applied using a 10 : 1 gear reduction handpiece 5 and 10 times on groups 4 and 5, respectively, with each application lasting 20 seconds. After etching with 37% phosphoric acid, composite resin was bonded. Thermocycling was performed and shear bond strength was measured. The following results were obtained : 1. Group 2 showed the highest bond strength, while group 3 showed the lowest, Shear bond strength decreased in the following order: 2>4>5>1>3. 2. Group 2 showed bond strength significantly higher compared to groups 1 and 3(p<0.05). 3. There were no significant differences between groups 2 and 3, which had been microabraded using HCl and pumice, and groups 4 and 5, to which PREMA had been applied, when bond strengths were compared(p>0.05). 4. When modes of fracture were examined, adhesive failure was observed in groups 3 and 4, while cohesive failure was observed in groups 1, 2, 3 and 4. Only mixed failures were found group 5. 5. When viewed using a SEM, groups 2 and 3, which had been microabraded using HCl and pumice, showed surface appearances similar to that of enamel etched with phosphoric acid. Groups 4 and 5, treated with PREMA, exhibited a smooth surface similar to that of group 1. All oops showed similar, typical surface characteristics following phosphoric acid etching.en
dc.language.isokoen
dc.publisher대한소아치과학회en
dc.subjectEnamel microabrasionen
dc.subjectComposite resinen
dc.subjectShear bond strengthen
dc.titleEnamel Microabrasion을 시행한 법랑질과 복합레진의 전단결합강도en
dc.typeArticleen
dc.contributor.AlternativeAuthorHong, Kee-Sang-
dc.contributor.AlternativeAuthorLee, Sang-Dae-
dc.contributor.AlternativeAuthorLee, Sang-Hoon-
Appears in Collections:
Files in This Item:

Altmetrics

Item View & Download Count

  • mendeley

Items in S-Space are protected by copyright, with all rights reserved, unless otherwise indicated.

Share